Grade | Density | Melting Point | Yield Strength (0.2%Offset) | Tensile Strength | Elongation |
Hastelloy C22 | 8.69 g/cm3 | 1399 °C (2550 °F) | Psi – 45000 , MPa – 310 | Psi – 1,00,000 , MPa – 690 | 45 % |
Hastelloy C276 | 8.89 g/cm3 | 1370 °C (2500 °F) | Psi – 52,000 , MPa – 355 | Psi – 1,15,000 , MPa – 790 | 40 % |
Hastelloy B2 | 9.2 g/cm3 | 1370 °C (2500 °F) | Psi – 51000 , MPa – 350 | Psi – 1,10,000 , MPa – 760 | 40 % |